01

Condensation and dripping

The most common — and most misunderstood — issue on site. Condensation is almost never "the material does not insulate", but something else.

Why does the pipe still drip even though it is insulated?
Condensation needs the surface to be below the air dew point. So check in three steps: ① Is the thickness enough (what indoor temperature and humidity were assumed? if humidity was taken too low, it will fall short); ② Is there a break — an unsealed joint, an untreated valve, flange or support where cold bridges leak out; ③ Was the material crushed or wetted during installation. The material can be thermally sound, but any gap leaks, and condensation forms at that point first.
Why are joints the most likely weak point?
Cold escapes fastest where nothing is sealed. A perfectly insulated pipe run still has a hole wherever a joint is not bonded tight. The correct method: full adhesive coating on both faces, then pressed together — no gap; and on foil-faced material, wrap a layer of foil tape over the seam as well. Two coats of glue plus tape is what actually seals it. This is where workmanship slips most on site, and where we watch hardest.
How should valves, flanges and tees be treated?
These are the easiest places to cut corners and the most likely to fail. The principle is to cut the material to the fitting’s shape and wrap it tight, not to piece offcuts on. Develop the fitting profile, cut the sheet to it, wrap with one piece where possible, bond layer by layer, then reinforce the seam with foil tape. Poor work here is often the source of the first drip in the whole system — and it is where a crew’s skill shows most.
Why does the same material leak on my site but not on others?
Most likely not a material difference but a site-condition difference: indoor humidity, whether joints were sealed, whether the work met wet weather. So when selecting, always give us the actual operating temperature and humidity — sizing to real conditions costs far less than thickening afterwards.
02

Thickness and selection

Thickness is not "thicker is safer" — it is calculated from the conditions. Too thin condenses; too thick wastes money.

What determines the thickness?
Three inputs: ① the media temperature in the pipe (chilled water, hot water, or ambient line); ② ambient temperature and relative humidity (this is the key one — a southern rainy season and a northern winter are entirely different); ③ whether anti-condensation is required (when it is, thickness is usually driven by the dew point, not by "insulation performance"). Sizing on media temperature alone is the root of many condensation cases.
What should be watched in humid southern regions?
A humid region has a higher dew point, so the thickness needed for anti-condensation is clearly larger and the sealing requirement is higher. The same A/C water system in Guangzhou and in the north can differ by a full size step when calculated for anti-condensation. So telling us the project city is not a courtesy — it is a necessary input.
Is thicker always better?
No. Beyond what anti-condensation needs, the extra cost buys almost nothing, while taking space and adding weight. What decides success is "enough + sealed tight"; enough thickness with a leaking joint still fails.
03

Fire rating

B1 is flame-retardant, not non-combustible. Understanding this avoids a lot of inspection disputes.

Does B1 mean it will not catch fire?
No. B1 (flame-retardant) means it is hard to ignite and self-extinguishes when the flame is removed. It is far safer than combustible material, but it is not non-combustible. Where a fire-resistance requirement applies (fire walls, fire-rated separation), B1 material cannot replace the corresponding fire construction — follow the design code.
A client asks "will it pass fire inspection" — what is the accurate answer?
Accurately: we supply the material's own combustion performance (GB 8624 B1) with the corresponding test report; whether a given location passes inspection depends on the design requirement and the whole construction, not on one material. Not promising a blanket "it will pass" is responsible to both sides.
04

Installation and site

Half of insulation performance is the material and half is the workmanship. Here is what we learned after hitting the traps.

How is adhesive applied correctly?
The key is "both faces, full coat, wait before joining". Coat both sides of the joint, evenly and fully, then let it flash off until tacky (not wet to the touch) before pressing together. Coating one side, joining immediately, or applying too thin all lead to weak joints that open up over time. We specify two-face glueing, never one.
When should you not install?
In wet weather, rain, or with free water on the surface, do not install directly — sealing moisture inside causes more problems later. Nor should wetted or damaged material be used "to get by". It may look like lost schedule, but it saves the rework.
The foil face creases easily in transit and installation — what do you do?
This is a problem we genuinely hit and genuinely solved. The root cause is not handling but the bond between foil and adhesive. We switched to better-suited foil and adhesive and brought in an automated laminating machine for a tighter, more even bond, reducing creasing at the source. See the full story →
Not finding it

Describe your problem to us

Symptom + scenario (media temperature, pipe diameter, environment, region) — the more specific, the more accurate we can be. If we cannot answer, we will look, ask and test until we give you an answer you can act on.

Leave your details and we will get back to you shortly (or just call / add us on WeChat).

In a hurry, call: +86 18666997135 · Overseas: WhatsApp